NASA's 3D-printed superalloy can take the heat
GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.
NASA's 3D-printed superalloy can take the heat
by Brian Newbacher for GRC News
Washington DC (SPX) Apr 24, 2023
NASA has demonstrated a breakthrough in 3D printable high-temperature materials that could lead to stronger, more durable parts for airplanes and spacecraft.

A team of innovators from NASA and The Ohio State University detailed the characteristics of the new alloy, GRX-810, in a peer-reviewed paper published in the journal Nature.

"This superalloy has the potential to dramatically improve the strength and toughness of components and parts used in aviation and space exploration," said Dr. Tim Smith of NASA's Glenn Research Center in Cleveland, lead author of the Nature paper. Smith and his Glenn colleague Christopher Kantzos invented GRX-810.

Smith and his team employed time-saving computer modeling, as well as a laser 3D printing process that fused metals together, layer-by-layer, to create the new alloy. They used this process to produce the NASA logo pictured above.

GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.

Current state-of-the-art 3D printed superalloys can withstand temperatures up to 2,000 degrees Fahrenheit. Compared to those, GRX-810 is twice as strong, over 1,000 times more durable, and twice as resistant to oxidation.

"This new alloy is a major achievement," said Dale Hopkins, deputy project manager of NASA's Transformational Tools and Technologies project. "In the very near future, it may well be one of the most successful technology patents NASA Glenn has ever produced."

A team of contributors from Glenn, NASA's Ames Research Center in California's Silicon Valley, NASA's Marshall Space Flight Center in Huntsville, Alabama, and The Ohio State University co-authored the Nature paper.

GRX-810 was developed under NASA's Transformational Tools and Technologies project, with support from the agency's Game Changing Development Program.

Related Links
Aeronautics at NASA
Space Technology News - Applications and Research

Subscribe Free To Our Daily Newsletters
Tweet

RELATED CONTENT
The following news reports may link to other Space Media Network websites.
TECH SPACE
SwRI joins new NASA institute to qualify, certify additive manufacturing methods
San Antonio TX (SPX) Apr 19, 2023
Southwest Research Institute will contribute to a new NASA institute to improve understanding and enable rapid certification of metal parts created using advanced additive manufacturing (AM) techniques. The Institute for Model-based Qualification and Certification of Additive Manufacturing (IMQCAM) will work to improve computer models of additively manufactured metal parts and expand their utility in spaceflight applications. Additive manufacturing uses 3D printing or rapid prototyping to build an ... read more

TECH SPACE
TECH SPACE
Curiosity: Move slowly and don't break things: Sols 3810-3811

NASA Retires Mineral Mapping Instrument on Mars Orbiter

China releases first panoramic images of Mars

Sols 3812-3813: Tiny Sticks Poking Out at Us

TECH SPACE
Fly me to the Moon: Firms lining up lunar landings

Wanted: new ideas to live off Moon resources

NASA extracts oxygen from lunar soil simulant

Radio silence suggests failure of Japan Moon landing

TECH SPACE
Juice's first taste of science from space

Icy Moonquakes: Surface Shaking Could Trigger Landslides

Europe's Jupiter probe launched

Europe's JUICE mission blasts off towards Jupiter's icy moons

TECH SPACE
UGA researchers discover new planet outside solar system

Scientists discover rare element in exoplanet's atmosphere

New stellar danger to planets identified by Chandra

TESS celebrates fifth year scanning the sky for new worlds

TECH SPACE
SpaceX delays launch of 46 Starlink satellites

SpaceX's Starship launch: successful failure of most powerful rocket in history

Aerojet Rocketdyne to provide propulsion for three additional Orion spacecraft

Potential Failure Modes of SpaceX's Starship

TECH SPACE
China to promote space science progress on five themes

China to develop satellite constellation for deep space exploration

China's space missions break new ground

Space exploration for betterment of humankind

TECH SPACE
SOHO chases asteroid's tail

Asteroid's comet-like tail is not made of dust, solar observatories reveal

What colour is an asteroid? Hyperspectral imager to find out

China to launch Tianwen 2 mission to explore asteroid

Subscribe Free To Our Daily Newsletters




The content herein, unless otherwise known to be public domain, are Copyright 1995-2026 - Space Media Network. All websites are published in Australia and are solely subject to Australian law and governed by Fair Use principals for news reporting and research purposes. AFP, UPI and IANS news wire stories are copyright Agence France-Presse, United Press International and Indo-Asia News Service. ESA news reports are copyright European Space Agency. All NASA sourced material is public domain. Additional copyrights may apply in whole or part to other bona fide parties. All articles labeled "by Staff Writers" include reports supplied to Space Media Network by industry news wires, PR agencies, corporate press officers and the like. Such articles are individually curated and edited by Space Media Network staff on the basis of the report's information value to our industry and professional readership. Advertising does not imply endorsement, agreement or approval of any opinions, statements or information provided by Space Media Network on any Web page published or hosted by Space Media Network. General Data Protection Regulation (GDPR) Statement Our advertisers use various cookies and the like to deliver the best ad banner available at one time. All network advertising suppliers have GDPR policies (Legitimate Interest) that conform with EU regulations for data collection. By using our websites you consent to cookie based advertising. If you do not agree with this then you must stop using the websites from May 25, 2018. Privacy Statement. Additional information can be found here at About Us.